Disordered rock-salt (DRX) cathodes within the Li–Mn–Ti–O (LMTO) composition space have recently been extensively studied, as they promise to deliver exceptional energy density at low cost in Li-ion batteries. The development of LMTO DRX with improved electrochemical performance requires optimization of the composition and particle size/morphology, which are determined by synthesis conditions such as annealing temperature. These challenges motivate an investigation of the LMTO rock-salt phase diagram, with a focus on understanding the stability of DRX by quantifying the order-disorder transition temperature (Tdisord) as a function of composition. First-principles calculations and X-ray diffraction experiments are applied to establish the LMTO phase diagram, which lies within the LiMnO2–Li2MnO3–Li2TiO3 pseudo-ternary. The Tdisord decreases significantly as off-stoichiometry is introduced to the end-point compositions, resulting in a eutectoid phase diagram. Importantly, a significant range of LMTO compositions containing small to moderate fractions of Li-excess and Ti4+ doping (relative to LiMnO2) have Tdisord spanning 700–900 °C. These temperatures are substantially lower than conventional DRX synthesis temperatures, suggesting the promise of decreasing synthesis temperatures for specific DRX compositions. The compositions containing moderate to high fractions of Mn4+ instead have greater Tdisord and phase separation to layered Li2MnO3 becomes highly favored.
Abstract:
Publication date:
July 21, 2026
Publication type:
Journal Article